The following competitors host bars were dragged for one mile:
| High carbon steel-carbide removed Standard wear rod Stainless steel Hard steel |
- Bottom Line - Sno Stuff - USI - USI |
The order of wear performance
based on our tests:
[The bar losing the least amount of material as
determined by weight]
|

"REALITY" It is not the carbide that wears out, but the host bar that erodes around the carbide until the carbide falls out. As our drag test shows, BERGSTROM rods out wear all others.